AWS: A5.5 (E7018-B2L)
Process: SMAW
Alloy Type: Low Alloy

Low alloy steel electrode for welding Cr-Mo steels, such as 1.5%Cr – 0.5%Mo and 0.5% Cr – 0.5% Mo. This electrode is recommended for high strength steels requiring tensile strength greater than 80 ksi, and for the fabrication of boilers and piping used in high-temperature service.

AWS MECHANICAL REQUIREMENTS (STRESS RELIEVED 1 HR AT 1275°F):

UTS (ksi)Yield (ksi)%El
755719