DevCor 70-S
AWS: A5.23 (ECG)
Process: SAW
Alloy Type: Low Alloy
A low hydrogen SAW wire for joining and repair of 0.5% Ni – 0.25% Mo steels. This wire exhibits great properties in the as welded condition, as well as with extended post-weld heat treat.
Typical Mechanical Properties (As Welded):
UTS (ksi) | Yield (ksi) | %El | CVN (ft/lbs) @ -60°F |
---|---|---|---|
98 | 87 | 20 | 120 |
Typical Mechanical Properties (Stress Relieved 10 hr at 1150°F):
UTS (ksi) | Yield (ksi) | %El | CVN (ft/lbs) @ -60°F |
---|---|---|---|
86 | 75 | 27 | 90 |